Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 290 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 290 [-] |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % |
Límite elástico | 23.0 °C | 530 MPa Show Supplier Material materials with Límite elástico of 530 MPa |
Resistencia a la tracción | 23.0 °C | 730 - 930 MPa Show Supplier Material materials with Resistencia a la tracción of 730 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Manganeso | 1.2 % Show Supplier Material materials with Manganeso of 1.2 % |
Molibdeno | 3 - 5 % Show Supplier Material materials with Molibdeno of 3 - 5 % |
Nitrógeno | 0.24 - 0.32 % Show Supplier Material materials with Nitrógeno of 0.24 - 0.32 % |
Níquel | 6 - 8 % Show Supplier Material materials with Níquel of 6 - 8 % |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % |
Silicona | 0.8 % Show Supplier Material materials with Silicona of 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Oil and gas, Marine |