Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 12 % Show Supplier Material materials with Elongación of 12 % |
Límite elástico | 23.0 °C | 550 MPa Show Supplier Material materials with Límite elástico of 550 MPa |
Resistencia a la tracción | 23.0 °C | 750 - 950 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.33 - 0.45 % Show Supplier Material materials with Carbono of 0.33 - 0.45 % |
Cromo | 15.5 - 17.5 % Show Supplier Material materials with Cromo of 15.5 - 17.5 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % |
Molibdeno | 0.8 - 1.3 % Show Supplier Material materials with Molibdeno of 0.8 - 1.3 % |
Níquel | 1 % Show Supplier Material materials with Níquel of 1 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automobile |