General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.45 g/cm³ Show Supplier Material materials with Densidad of 7.45 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 183 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 183 [-] | HBW 10/3000 |
Dureza Rockwell B | 23.0 °C | 90 [-] Show Supplier Material materials with Dureza Rockwell B of 90 [-] | |
Elongación A5 | 23.0 °C | 18 % Show Supplier Material materials with Elongación A5 of 18 % | |
Energía de impacto Charpy | 23.0 °C | 19 J Show Supplier Material materials with Energía de impacto Charpy of 19 J | |
Energía de impacto Izod | 23.0 °C | 27 J Show Supplier Material materials with Energía de impacto Izod of 27 J | |
Estricción | 23.0 °C | 20 % Show Supplier Material materials with Estricción of 20 % | |
Límite elástico Rp0.5 | 23.0 °C | 282 MPa Show Supplier Material materials with Límite elástico Rp0.5 of 282 MPa | |
Límite proporcional en compresión | 23.0 °C | 207 MPa Show Supplier Material materials with Límite proporcional en compresión of 207 MPa | |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa | |
Resistencia a la compresión | 23.0 °C | 956 MPa Show Supplier Material materials with Resistencia a la compresión of 956 MPa | |
Resistencia a la fatiga | 23.0 °C | 228 MPa Show Supplier Material materials with Resistencia a la fatiga of 228 MPa | 100.000.000 cycles |
Resistencia a la tracción | 23.0 °C | 724 MPa Show Supplier Material materials with Resistencia a la tracción of 724 MPa | |
Resistencia al cizallamiento | 23.0 °C | 400 MPa Show Supplier Material materials with Resistencia al cizallamiento of 400 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Calor específico of 420 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Conductividad térmica | 23.0 °C | 63 W/(m·K) Show Supplier Material materials with Conductividad térmica of 63 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 8.00E+6 S/m |
Specific Electrical conductivity | 14 % IACS Show Supplier Material materials with Specific Electrical conductivity of 14 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | This alloy is well suited for use as gears, worm wheels, bushings and bearings. The machine tool industry has adopted AMPCO® 18 as standard for all applications requiring good sliding properties, wear resistance, fatigue resistance, toughness and/or resistance to deformation under load. AMPCO® 18 is used in steel mill service as screw down nuts, slippers (many of which are "cast to size"), gears, wedges and breaker blocks. AMPCO® 18 has an excellent corrosion resistance and is used in pickling service for such parts as hooks, crates and spreaders, etc. |