General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.06 g/cm³ Show Supplier Material materials with Densidad of 7.06 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 331 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 331 [-] | HBW 10/3000 |
Dureza Rockwell C | 23.0 °C | 35 [-] Show Supplier Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A5 | 23.0 °C | 0.5 % Show Supplier Material materials with Elongación A5 of 0.5 % | |
Energía de impacto Charpy | 23.0 °C | 2.7 J Show Supplier Material materials with Energía de impacto Charpy of 2.7 J | |
Energía de impacto Izod | 23.0 °C | 2.7 J Show Supplier Material materials with Energía de impacto Izod of 2.7 J | |
Estricción | 23.0 °C | 0 % Show Supplier Material materials with Estricción of 0 % | |
Límite elástico Rp 0,2 | 23.0 °C | 489 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 489 MPa | |
Límite elástico a la compresión, 0,1% | 23.0 °C | 620 MPa Show Supplier Material materials with Límite elástico a la compresión, 0,1% of 620 MPa | |
Módulo elástico | 23.0 °C | 103 GPa Show Supplier Material materials with Módulo elástico of 103 GPa | |
Resistencia a la compresión | 23.0 °C | 1379 MPa Show Supplier Material materials with Resistencia a la compresión of 1379 MPa | |
Resistencia a la tracción | 23.0 °C | 586 MPa Show Supplier Material materials with Resistencia a la tracción of 586 MPa | |
Resistencia al cizallamiento | 23.0 °C | 414 MPa Show Supplier Material materials with Resistencia al cizallamiento of 414 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Calor específico of 420 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K |
Conductividad térmica | 23.0 °C | 42 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 6.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 6.00E+6 S/m |
Specific Electrical conductivity | 10 % IACS Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | The field of service of AMPCO® 22, with few exceptions, is limited to forming and/or drawing stainless steel, especially when runs are long or gauge is heavy and it is essential that tolerances are maintained. |