General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 187 [-] Show Supplier Material materials with Dureza Brinell of 187 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 22 % Show Supplier Material materials with Estricción of 22 % | |
Límite elástico | 23.0 °C | 400 MPa Show Supplier Material materials with Límite elástico of 400 MPa | |
Resistencia a la tracción | 23.0 °C | 683 MPa Show Supplier Material materials with Resistencia a la tracción of 683 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 8.5 - 9.5 % Show Supplier Material materials with Aluminio of 8.5 - 9.5 % | ||
Cobre | Balance, including silver | ||
Hierro | 3 - 6 % Show Supplier Material materials with Hierro of 3 - 6 % | ||
Manganeso | 0.5 - 3.5 % Show Supplier Material materials with Manganeso of 0.5 - 3.5 % | ||
Níquel | 4 - 6 % Show Supplier Material materials with Níquel of 4 - 6 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 1.5 % Show Supplier Material materials with Silicona of 1.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Ship fittings, Propeller gear housings, Power plant valves, Marine propulsion systems, Intake screens, Ship propellers, Welding AMPCO® 45, Piping systems, Welding AMPCO® 483, Oil recovery pumps |