General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.05 % Show Supplier Material materials with Absorción de agua of 0.03 - 0.05 % | ASTM D570 | |||
Coefficient of friction | 0.33 [-] Show Supplier Material materials with Coefficient of friction of 0.33 [-] | ASTM D1894 | vs Steel, Static | |
0.33 [-] Show Supplier Material materials with Coefficient of friction of 0.33 [-] | ASTM D1894 | vs Steel, Kinetic | ||
Densidad | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 75 % Show Supplier Material materials with Índice límite de óxigeno of 75 % | ASTM D2863, ISO 4589-1/-2 | dry |
Mecánica
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Dureza Shore D | 60 - 70 [-] Show Supplier Material materials with Dureza Shore D of 60 - 70 [-] | ASTM D2240 | |||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal | |
100 - 300 % Show Supplier Material materials with Elongación of 100 - 300 % | ASTM D638 | ||||
Elongation at yield | 14.5 % Show Supplier Material materials with Elongation at yield of 14.5 % | ISO 527-1/-2 | dry | ||
15 - 25 % Show Supplier Material materials with Elongation at yield of 15 - 25 % | ASTM D638 | ||||
Impact strength, Charpy notched, ASTM | 23 °C | 534 - 1070 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 534 - 1070 J/m | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | |||
Límite elástico | 12 MPa Show Supplier Material materials with Límite elástico of 12 MPa | ISO 527-1/-2 | dry | ||
20 - 34.5 MPa Show Supplier Material materials with Límite elástico of 20 - 34.5 MPa | ASTM D638 | ||||
Módulo de flexión | 0.483 - 0.758 GPa Show Supplier Material materials with Módulo de flexión of 0.483 - 0.758 GPa | ASTM D790 | |||
Módulo elástico | 0.552 - 0.896 GPa Show Supplier Material materials with Módulo elástico of 0.552 - 0.896 GPa | ASTM D638 | |||
0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | ISO 527-1/-2 | dry | |||
Resistencia a la compresión | 31 - 41.4 MPa Show Supplier Material materials with Resistencia a la compresión of 31 - 41.4 MPa | ASTM D695 | |||
Resistencia a la flexión | 20.7 - 34.5 MPa Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | ||
Resistencia a la tracción | 20 - 27.6 MPa Show Supplier Material materials with Resistencia a la tracción of 20 - 27.6 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000126 - 0.000185 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 - 0.000185 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Temperatura de flexión bajo carga | 40 - 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 40 - 55 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
60 - 75 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 - 75 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Temperatura de fusión | 140 - 145 °C Show Supplier Material materials with Temperatura de fusión of 140 - 145 °C | ASTM D3418 | |||||||
143 °C Show Supplier Material materials with Temperatura de fusión of 143 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -41.1 - -39.4 °C Show Supplier Material materials with Temperatura de transición del vidrio of -41.1 - -39.4 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 3.5 - 10.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 - 10.6 [-] | 1KHz | ASTM D150 | |
Factor de disipación | 0.02 - 0.21 [-] Show Supplier Material materials with Factor de disipación of 0.02 - 0.21 [-] | 100KHz | ASTM D150 | |
Rigidez dieléctrica | 51.2 - 59.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 51.2 - 59.1 kV/mm | ASTM D149 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 6 - 1200 Pa·s Show Supplier Material materials with Melt viscosity of 6 - 1200 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 4 - 21 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4 - 21 g/10min | ASTM D1238 | 230°C/3.8kg | |
Velocidad de flujo del volumen derretido | 9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | ISO 1133 | dry | 232°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Cables,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables |