General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Abrasion resistance | 41 mm³ Show Supplier Material materials with Abrasion resistance of 41 mm³ | dry | ISO 4649 |
Absorción de agua | 1.43 % Show Supplier Material materials with Absorción de agua of 1.43 % | Sim. to ISO 62 | |
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.76 % Show Supplier Material materials with Moisture absorption of 0.76 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | cond. | ISO 527-1/-2 | ||
22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | |||
Límite elástico | 22 MPa Show Supplier Material materials with Límite elástico of 22 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.39 GPa Show Supplier Material materials with Módulo elástico of 0.39 GPa | cond. | ISO 527-1/-2 | ||
0.414 GPa Show Supplier Material materials with Módulo elástico of 0.414 GPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 120 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 120 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 172 °C Show Supplier Material materials with Temperatura de fusión of 172 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 129 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 129 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: Extrusion: |