Límite elástico: 22 MPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-20

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2821-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2801-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2751-00

Suministrada por:

Arkema: High Performance Polymers

1000 Series

EN 573-3 Grade AW-1050A O

Suministrada por:

2 proveedores de Matmatch

1000 Series

EN 573-3 Grade AW-1050A O

Suministrada por:

2 proveedores de Matmatch

1000 Series

EN 573-3 Grade AW-1050A H111

Suministrada por:

2 proveedores de Matmatch

1000 Series

EN 573-3 Grade AW-1050A H111

Suministrada por:

2 proveedores de Matmatch

1000 Series

EN 573-3 Grade AW-1080A O

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1080A O

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1080A H111

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1080A H111

Suministrada por:

1 proveedor Matmatch

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2900-04

Suministrada por:

Arkema: High Performance Polymers

Poliamida termoplástica

Pebax® 6333 SP 01

Suministrada por:

Arkema: High Performance Polymers

Copoliéster termoplástico

Hytrel® HTR8241

High Molecular Weight Polyethylene (PE-HMW)

HMWPE ISO-TECH

Suministrada por:

ISO-TECH Kunststoff GmbH

Poliamida termoplástica

Pebax® 7033 SA 01 MED

Suministrada por:

Arkema: High Performance Polymers

Poliamida termoplástica

Pebax® 7033 SA 01

Suministrada por:

Arkema: High Performance Polymers
Página 1 de 2