General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 2 % Show Supplier Material materials with Absorción de agua of 2 % | Sim. to ISO 62 | |
Bio-based content | 90 % Show Supplier Material materials with Bio-based content of 90 % | ||
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | Sim. to ISO 62 | |
Índice límite de óxigeno | 33 % Show Supplier Material materials with Índice límite de óxigeno of 33 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 69 [-] Show Supplier Material materials with Dureza Shore D of 69 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | cond., dry | ISO 527-1/-2 | ||
Módulo elástico | 1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 38 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 38 kJ/m² | cond. | ISO 179/1eU | |
23 °C | 83 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 83 kJ/m² | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.000102 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000102 1/K | dry | ISO 11359-1/-2 | ||||
Temperatura de fusión | 189 °C Show Supplier Material materials with Temperatura de fusión of 189 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 IEC 60695-11-10: V-0 and yellow card available |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | dry | 100Hz | IEC 60250 | |
3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | dry | 1MHz | IEC 60250 | ||
Factor de disipación | 0.018 [-] Show Supplier Material materials with Factor de disipación of 0.018 [-] | dry | 1MHz | IEC 60250 | |
0.0221 [-] Show Supplier Material materials with Factor de disipación of 0.0221 [-] | dry | 100Hz | IEC 60250 | ||
Rigidez dieléctrica | 28 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 28 kV/mm | cond., dry | IEC 60243-1 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | cond. | IEC 60093 | min. | |
1e+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm | dry | IEC 60093 | |||
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | Transverse | |
Velocidad de flujo del volumen derretido | 95 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 95 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry - Injection Molding,Automotive Cables,Performance Wire | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |