Resistencia al choque, ensayo Charpy no entallado: 38 kJ/m²

Quick Comparison

Polyamide 11 (PA11)

Rilsan® MB 3000 NAT

Suministrada por:

Arkema: High Performance Polymers

Polyamide 6T (PA6T)

Zytel® HTNFG52G35HSL BK011

Tereftalato de polibutileno (PBT)

EPIMIX PBT GFR 30 NC Q1D0A301

Suministrada por:

EPSAN

Tereftalato de polibutileno (PBT)

Crastin® SK692FR NC010

Polyamide 6 (PA6)

Novamid® 1010G30 NA

Suministrada por:

DSM Engineering Materials

Other Polyamide (PA)

Rilsan® HT CMNO

Suministrada por:

Arkema: High Performance Polymers

Polipropileno

ALFACOM® 50HVL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 50HVH

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 50CRL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 50CRH

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 40HVL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 40HVH

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 40CRL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 40CRH

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 30HVL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 30HVH

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 30CRL

Suministrada por:

Green World Compounding

Polipropileno

ALFACOM® 30CRH

Suministrada por:

Green World Compounding