General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 60 % Show Supplier Material materials with Bio-based content of 60 % | ||
Densidad | 1.31 g/cm³ Show Supplier Material materials with Densidad of 1.31 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Módulo elástico | 8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 89 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 89 kJ/m² | dry | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 222 °C Show Supplier Material materials with Temperatura de fusión of 222 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 217 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 217 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |