General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 99 % Show Supplier Material materials with Bio-based content of 99 % | ||
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Límite elástico | 29 MPa Show Supplier Material materials with Límite elástico of 29 MPa | cond. | ISO 527-1/-2 | |
Módulo elástico | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 202 °C Show Supplier Material materials with Temperatura de fusión of 202 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments |