General
Medidas
Property | Value |
---|---|
Espesor | 6 - 575 mm Show Supplier Material materials with Espesor of 6 - 575 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 20 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 20 [-] |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % |
Límite elástico | 23.0 °C | 28 MPa Show Supplier Material materials with Límite elástico of 28 MPa |
Módulo de cizallamiento | 23.0 °C | 25.9 GPa Show Supplier Material materials with Módulo de cizallamiento of 25.9 GPa |
Módulo elástico | 23.0 °C | 69 GPa Show Supplier Material materials with Módulo elástico of 69 GPa |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Calor específico of 900 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 2.35E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.35E-5 1/K | Mean values between 20°C and the mentioned temperature |
200.0 °C | 2.44E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.44E-5 1/K | Mean values between 20°C and the mentioned temperature | |
300.0 °C | 2.54E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.54E-5 1/K | Mean values between 20°C and the mentioned temperature | |
Conductividad térmica | 23.0 °C | 210 - 220 W/(m·K) Show Supplier Material materials with Conductividad térmica of 210 - 220 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 3.40E+7 - 3.60E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 3.40E+7 - 3.60E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % | ||
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % | ||
Magnesio | 0.05 % Show Supplier Material materials with Magnesio of 0.05 % | ||
Manganeso | 0.05 % Show Supplier Material materials with Manganeso of 0.05 % | ||
Otro | 0.03 % Show Supplier Material materials with Otro of 0.03 % | Single | |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % | ||
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % | ||
Zinc | 0.07 % Show Supplier Material materials with Zinc of 0.07 % |
Technological properties
Property | ||
---|---|---|
Anodizing | very good | |
Application areas | Electronics industry; Semiconductor industry; Panelling in machine construction and plant construction; Parts with a decorative surface; Automotive parts; Food industry | |
Corrosion properties | good | |
Dimensional stability | very good | |
General machinability | very good | |
Soldering general | very good | |
Welding | Gas: good, WIG: good |