General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Densidad of 2.66 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 5 - 500 mm Show Supplier Material materials with Espesor of 5 - 500 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 70 - 80 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 70 - 80 [-] | |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | A10 mm |
Límite elástico | 23.0 °C | 110 - 130 MPa Show Supplier Material materials with Límite elástico of 110 - 130 MPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 230 - 290 MPa Show Supplier Material materials with Resistencia a la tracción of 230 - 290 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Calor específico of 900 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 2.35E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.35E-5 1/K | Mean values between 20°C and the mentioned temperature |
Conductividad térmica | 23.0 °C | 110 - 140 W/(m·K) Show Supplier Material materials with Conductividad térmica of 110 - 140 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.60E+7 - 1.80E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | ||
Cromo | 0.05 - 0.25 % Show Supplier Material materials with Cromo of 0.05 - 0.25 % | ||
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % | ||
Magnesio | 4 - 4.9 % Show Supplier Material materials with Magnesio of 4 - 4.9 % | ||
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % | ||
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | Total | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | ||
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % | ||
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | very good | |
Application areas | Tool making, mould making and model making; Laser technology; Cover plates; Printing technology; Fixture construction; Electronics and optical industry; Packaging technology; Medical technology | |
Corrosion properties | very good | |
Dimensional stability | very good | |
General machinability | very good | |
Welding | WIG: good, MIG: good, Resistance welding: good |