General
Medidas
Property | Value |
---|---|
Espesor | 8 - 100 mm Show Supplier Material materials with Espesor of 8 - 100 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 126 - 140 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 126 - 140 [-] |
Elongación | 23.0 °C | 5 - 6 % Show Supplier Material materials with Elongación of 5 - 6 % |
Elongación A50 | 23.0 °C | 7 % Show Supplier Material materials with Elongación A50 of 7 % |
Límite elástico | 23.0 °C | 340 - 390 MPa Show Supplier Material materials with Límite elástico of 340 - 390 MPa |
Módulo elástico | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo elástico of 72 GPa |
Resistencia a la tracción | 23.0 °C | 430 - 475 MPa Show Supplier Material materials with Resistencia a la tracción of 430 - 475 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Calor específico of 862 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 2.34E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.34E-5 1/K | Mean values between 20°C and the mentioned temperature |
200.0 °C | 2.43E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.43E-5 1/K | Mean values between 20°C and the mentioned temperature | |
300.0 °C | 2.52E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.52E-5 1/K | Mean values between 20°C and the mentioned temperature | |
Conductividad térmica | 23.0 °C | 130 - 160 W/(m·K) Show Supplier Material materials with Conductividad térmica of 130 - 160 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.90E+7 - 2.30E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 1.2 - 2 % Show Supplier Material materials with Cobre of 1.2 - 2 % | ||
Cromo | 0.18 - 0.28 % Show Supplier Material materials with Cromo of 0.18 - 0.28 % | ||
Hierro | 0.5 % Show Supplier Material materials with Hierro of 0.5 % | ||
Magnesio | 2.1 - 2.9 % Show Supplier Material materials with Magnesio of 2.1 - 2.9 % | ||
Manganeso | 0.3 % Show Supplier Material materials with Manganeso of 0.3 % | ||
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | Total | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | ||
Titanio | 0.2 % Show Supplier Material materials with Titanio of 0.2 % | ||
Zinc | 5.1 - 6.1 % Show Supplier Material materials with Zinc of 5.1 - 6.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | moderate | |
Application areas | Tool making, mould making and model making; Aerospace; Military technology | |
Corrosion properties | moderate | |
General machinability | good | |
Soldering general | not recommended | |
Welding | Resistance welding: good |