Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 1428 [-] Show Supplier Material materials with Dureza Vickers of 1428 [-] | converted from GPa |
Módulo elástico | 23.0 °C | 220 GPa Show Supplier Material materials with Módulo elástico of 220 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 6.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6.5 MPa·√m | |
Resistencia a la compresión | 23.0 °C | 2300 MPa Show Supplier Material materials with Resistencia a la compresión of 2300 MPa | |
Resistencia a la flexión | 23.0 °C | 1000 MPa Show Supplier Material materials with Resistencia a la flexión of 1000 MPa | 4-point bending flexural test |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.00E+9 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+9 Ω·m |
600.0 °C | 10000 Ω·m Show Supplier Material materials with Resistividad eléctrica of 10000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Bearings and guide parts for machine engineering Medical implants | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Ceramic Injection Molding (CIM) |