General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 1733 [-] Show Supplier Material materials with Dureza Vickers of 1733 [-] | converted from GPa |
Módulo elástico | 23.0 °C | 360 GPa Show Supplier Material materials with Módulo elástico of 360 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 5 MPa·√m | |
Resistencia a la compresión | 23.0 °C | 2600 MPa Show Supplier Material materials with Resistencia a la compresión of 2600 MPa | |
Resistencia a la flexión | 23.0 °C | 600 MPa Show Supplier Material materials with Resistencia a la flexión of 600 MPa | 4-point bending flexural test |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9E-6 1/K |
Conductividad térmica | 23.0 °C | 25 W/(m·K) Show Supplier Material materials with Conductividad térmica of 25 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.00E+14 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+14 Ω·m |
600.0 °C | 1000000 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1000000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting materials for machine Valves, gear wheels Sensors For highest mechanical loads | |
Other | *depending on the processing status of the injection molding or pressing tool | |