General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 510 [-] Show Supplier Material materials with Dureza Vickers of 510 [-] | converted from GPa |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa | |
Resistencia a la compresión | 23.0 °C | 900 MPa Show Supplier Material materials with Resistencia a la compresión of 900 MPa | |
Resistencia a la flexión | 23.0 °C | 140 MPa Show Supplier Material materials with Resistencia a la flexión of 140 MPa | 4-point bending flexural test |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.00E+11 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+11 Ω·m |
600.0 °C | 100000 Ω·m Show Supplier Material materials with Resistividad eléctrica of 100000 Ω·m | |
Technological properties
Property | ||
---|---|---|
Application areas | Isolators and fuses High frequency technology Especially used in the electronics and automotive industry | |
Other | *depending on the processing status of the injection molding or pressing tool | |
Processing history | Axial Pressing |