General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 0.9509 g/cm³ Show Supplier Material materials with Densidad of 0.9509 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 62 [-] Show Supplier Material materials with Dureza Shore D of 62 [-] | |
Elongación | 23.0 °C | 700 % Show Supplier Material materials with Elongación of 700 % | |
Módulo de flexión | 23.0 °C | 0.8 GPa Show Supplier Material materials with Módulo de flexión of 0.8 GPa | Min. |
Resistencia a la tracción | 23.0 °C | 26 MPa Show Supplier Material materials with Resistencia a la tracción of 26 MPa |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Brittleness temperature | -70 °C Show Supplier Material materials with Brittleness temperature of -70 °C | Max. |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al aislamiento superficial | 23.0 °C | 1.00E+16 Ω·cm² Show Supplier Material materials with Resistencia al aislamiento superficial of 1.00E+16 Ω·cm² | Min., GOST 50499 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 0.3 - 0.7 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 0.3 - 0.7 g/10min | GOST 11645, 190°С/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | METALEN PE-11K is used in the cable manufacture as a jacket of power cables and optical communication cables. | |
Processing methods | Temperature profile: Zone 1: 140°С, Zone 2: 150°С, Zone 3: 170°С, Zone 4: 180°С, Die plate: 200°С. |