Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
BS C110 / Cu-OFE Oxygen-free Copper
C110 (Cu-OFE) is the purest grade of oxygen-free copper, with a 99.99% copper content. With much tighter limits on impurities than other grades, C110 offers the highest electrical and thermal conductivity values available from a commercially available copper alloy and is not susceptible to embrittlement when hardened. Specified for electronic applications requiring freedom from harmful impurities and oxide which can impair and contaminate electronic devices, C110 also has high ductility. It shows the following features and properties:
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Suppliers with similar grades
Healthcare
Equipos médicos
Equipos radiográficos
Sistemas de fluido
Tecnología de aspirado
Fabricación
Soldadura
Sellos vidrio-metal
Tratamiento de superficies y revestimiento
Ánodos
Industria química
Equipamiento para la industria química
Intercambiadores de calor
Energía
Celdas de combustible
Ingeniería eléctrica
Semiconducting Materials
Componentes para equipos eléctricos
Componentes magnéticos
Accesorios eléctricos
Interruptores
Electrónica
Tubos electrónicos
Comunicaciones
Telecom Accessories
Waveguides
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value | Comment |
---|---|---|
Cobre | 99.99 % Show Material materials with Cobre of 99.99 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | General: Components for vacuum devices, switches, interrupters, deposition units, components for superconductive magnets, electron tubes including anodes, fins and collectors, glass-to-metal seals, wave guide tubes and linear accelerators | |
Cold Forming | Easily cold worked |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.