Description

2.4668 (NiCr19NbMo) is a precipitation hardening nickel-chromium alloy that also contains additions of iron, niobium, molybdenum, aluminium and titanium, providing a unique combination of high strength and corrosion resistance together with excellent weldability. It shows the following features and properties:


  • Excellent tensile, fatigue, creep and rupture strengths across a wide temperature range from around -253ºC to 705ºC
  • Excellent oxidation resistance, up to temperatures of around 980ºC due to the high chromium content
  • Outstanding corrosion resistance in many environments including organic and inorganic acids, other than when strongly oxidising, hydrogen sulphide and sour gases
  • Especially resistant to chloride stress-corrosion cracking
  • Exceptional weldability
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyTemperatureValue

    Densidad

    23.0 °C

    8.22 g/cm³

    Show Material materials with Densidad of 8.22 g/cm³

    Mecánica

    PropertyTemperatureValue

    Dureza Brinell

    23.0 °C

    313 - 354 [-]

    Show Material materials with Dureza Brinell of 313 - 354 [-]

    Elongación

    23.0 °C

    12 - 17 %

    Show Material materials with Elongación of 12 - 17 %

    Estricción

    23.0 °C

    15 %

    Show Material materials with Estricción of 15 %

    Límite elástico Rp 0,2

    23.0 °C

    827 - 1034 MPa

    Show Material materials with Límite elástico Rp 0,2 of 827 - 1034 MPa

    Módulo elástico

    23.0 °C

    204 GPa

    Show Material materials with Módulo elástico of 204 GPa

    Resistencia a la tracción

    23.0 °C

    1034 - 1276 MPa

    Show Material materials with Resistencia a la tracción of 1034 - 1276 MPa

    Aplicaciones térmicas

    PropertyTemperatureValueComment

    Coeficiente de dilatación térmica

    23.0 °C

    1.35E-5 1/K

    Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K

    Conductividad térmica

    23.0 °C

    14.2 W/(m·K)

    Show Material materials with Conductividad térmica of 14.2 W/(m·K)

    for 0-200°C

    Temperatura de fusión

    1260 - 1335 °C

    Show Material materials with Temperatura de fusión of 1260 - 1335 °C

    Magnético

    PropertyTemperatureValue

    Permeabilidad magnética relativa

    23.0 °C

    1 [-]

    Show Material materials with Permeabilidad magnética relativa of 1 [-]

    Chemical properties

    PropertyValue

    Aluminio

    0.5 %

    Show Material materials with Aluminio of 0.5 %

    Cromo

    19 %

    Show Material materials with Cromo of 19 %

    Hierro

    18 - 18.5 %

    Show Material materials with Hierro of 18 - 18.5 %

    Molibdeno

    3 %

    Show Material materials with Molibdeno of 3 %

    Niobio

    5 %

    Show Material materials with Niobio of 5 %

    Níquel

    53 %

    Show Material materials with Níquel of 53 %

    Titanio

    0.9 %

    Show Material materials with Titanio of 0.9 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Aerospace: Jet engine components, rocket motors and thrust reversers;Power generation: Nuclear reactor parts, gas turbine components, nuclear fuel element spacers, containment vessels and valves;Other: Hot extrusion tooling

    Corrosion properties

    Excellent corrosion resistance

    Hot forming

    It can be hot worked between 985-1150°C.