Medidas
Property | Value |
---|---|
Ancho | 700 - 1010 mm Show Supplier Material materials with Ancho of 700 - 1010 mm |
Espesor | 15 - 225 mm Show Supplier Material materials with Espesor of 15 - 225 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 280 - 325 [-] Show Supplier Material materials with Dureza Brinell of 280 - 325 [-] | as-delivered condition |
Dureza Rockwell C | 30 - 48 [-] Show Supplier Material materials with Dureza Rockwell C of 30 - 48 [-] | |
Resistencia a la tracción | 950 - 1095 MPa Show Supplier Material materials with Resistencia a la tracción of 950 - 1095 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Supplier Material materials with Azufre of 0.05 % |
Carbono | 0.33 % Show Supplier Material materials with Carbono of 0.33 % |
Cromo | 16 % Show Supplier Material materials with Cromo of 16 % |
Hierro | Balance |
Manganeso | 1.2 % Show Supplier Material materials with Manganeso of 1.2 % |
Níquel | 0.5 % Show Supplier Material materials with Níquel of 0.5 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mould frames, plastic moulds without special demands on surface quality. | |
Heat Treatment | Soft annealing: 850-880°C (Cooling in furnace) - Hardening: 1000-1050°C and quenching in oil |