Medidas
Property | Value |
---|---|
Diámetro | 232 - 532 mm Show Supplier Material materials with Diámetro of 232 - 532 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 230 [-] Show Supplier Material materials with Dureza Brinell of 230 [-] | soft annealed |
Dureza Rockwell C | 46 - 52 [-] Show Supplier Material materials with Dureza Rockwell C of 46 - 52 [-] | |
Resistencia a la tracción | 1485 - 1775 MPa Show Supplier Material materials with Resistencia a la tracción of 1485 - 1775 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 1.8 % Show Supplier Material materials with Cromo of 1.8 % |
Hierro | Balance |
Manganeso | 0.8 % Show Supplier Material materials with Manganeso of 0.8 % |
Molibdeno | 0.3 % Show Supplier Material materials with Molibdeno of 0.3 % |
Níquel | 0.6 % Show Supplier Material materials with Níquel of 0.6 % |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % |
Vanadio | 0.2 % Show Supplier Material materials with Vanadio of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Forging dies, extrusion press tools, compression moulding dies | |
Heat Treatment | Soft annealing: 780-800°C (Cooling in furnace or air) - Hardening: 880-920°C and quenching in air, oil or hot bath T=500-550°C | |
Welding | Outstanding weldability |