Medidas
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 230 [-] Show Supplier Material materials with Dureza Brinell of 230 [-] | soft annealed |
Dureza Rockwell C | 42 - 52 [-] Show Supplier Material materials with Dureza Rockwell C of 42 - 52 [-] | |
Resistencia a la tracción | 1320 - 1775 MPa Show Supplier Material materials with Resistencia a la tracción of 1320 - 1775 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.13e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.13e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.19e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.19e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.22e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.22e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.26e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.26e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.3e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.33e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.33e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.35e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.35e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 31.4 W/(m·K) Show Supplier Material materials with Conductividad térmica of 31.4 W/(m·K) | |
350 °C | 35.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 35.2 W/(m·K) | ||
700 °C | 36.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 36.2 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 3 % Show Supplier Material materials with Cromo of 3 % |
Hierro | Balance |
Manganeso | 0.3 % Show Supplier Material materials with Manganeso of 0.3 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Vanadio | 1 % Show Supplier Material materials with Vanadio of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | For use at highest temperatures, highly wear-exposed die inserts, high speed forging machines, casting dies for heavy metal processing | |
Heat Treatment | Soft annealing: 750-800°C (Cooling in furnace) - Hardening: 1070-1100°C and quenching in air, oil or hot bath T=500-550°C |