Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 230 [-] Show Supplier Material materials with Dureza Brinell of 230 [-] | soft annealed |
Dureza Rockwell C | 50 - 58 [-] Show Supplier Material materials with Dureza Rockwell C of 50 - 58 [-] | |
Resistencia a la tracción | 1665 - 2180 MPa Show Supplier Material materials with Resistencia a la tracción of 1665 - 2180 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.59 % Show Supplier Material materials with Carbono of 0.59 % |
Cromo | 1 % Show Supplier Material materials with Cromo of 1 % |
Hierro | Balance |
Manganeso | 0.9 % Show Supplier Material materials with Manganeso of 0.9 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for hand chisels of all types, including flat, cross-cut and pointed chisels for the treatment of hard materials; also for screwdrivers and other hand tools | |
Heat Treatment | Soft annealing: 710-740°C (Cooling in furnace) - Stress-relief-annealing: 650-680°C, Hardening: 810-850°C and quenching in oil |