Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 219 [-] Show Supplier Material materials with Dureza Brinell of 219 [-] | soft annealed |
Dureza Rockwell C | 50 - 57 [-] Show Supplier Material materials with Dureza Rockwell C of 50 - 57 [-] | |
Resistencia a la tracción | 1665 - 2105 MPa Show Supplier Material materials with Resistencia a la tracción of 1665 - 2105 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 1.35 % Show Supplier Material materials with Cromo of 1.35 % |
Hierro | Balance |
Manganeso | 0.65 % Show Supplier Material materials with Manganeso of 0.65 % |
Silicona | 1.35 % Show Supplier Material materials with Silicona of 1.35 % |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pneumatic chipping hammers, punching tools, riveting hammers, punches and woodworking tools | |
Heat Treatment | Soft annealing: 710-740°C (Cooling in furnace) - Stress-relief-annealing: 650-680°C, Hardening: 860-890°C and quenching in oil |