Medidas
Property | Value |
---|---|
Diámetro | 20 - 758 mm Show Supplier Material materials with Diámetro of 20 - 758 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 250 [-] Show Supplier Material materials with Dureza Brinell of 250 [-] | soft annealed |
Dureza Rockwell C | 56 - 62 [-] Show Supplier Material materials with Dureza Rockwell C of 56 - 62 [-] |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.05e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.05e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.19e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.19e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.22e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.22e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 16.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 16.7 W/(m·K) | |
350 °C | 20.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 20.5 W/(m·K) | ||
700 °C | 24.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 24.2 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 1.55 % Show Supplier Material materials with Carbono of 1.55 % |
Cromo | 12 % Show Supplier Material materials with Cromo of 12 % |
Hierro | Balance |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % |
Molibdeno | 0.75 % Show Supplier Material materials with Molibdeno of 0.75 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Vanadio | 0.9 % Show Supplier Material materials with Vanadio of 0.9 % |
Technological properties
Property | ||
---|---|---|
Application areas | Threading rolls and dies, cold extrusion tools, trimming, cutting and stamping tools, precision cutting tools, cold pilger mandrels, rotary shear blades, deep-drawing tools, highly wear-resistant plastic moulds | |
Heat Treatment | Soft annealing: 830-860°C (Cooling in furnace) - Stress-relief-annealing: 650-700°C (cooling in Furnace), Hardening: 1000-1050°C and quenching in oil, air or salt bath: 500-550°C |