Medidas
Property | Value |
---|---|
Diámetro | 12 - 302 mm Show Supplier Material materials with Diámetro of 12 - 302 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 230 [-] Show Supplier Material materials with Dureza Brinell of 230 [-] | soft annealed |
Dureza Rockwell C | 54 - 61 [-] Show Supplier Material materials with Dureza Rockwell C of 54 - 61 [-] |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20 °C | 33.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 33.5 W/(m·K) |
350 °C | 32 W/(m·K) Show Supplier Material materials with Conductividad térmica of 32 W/(m·K) | |
700 °C | 30.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30.9 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.95 % Show Supplier Material materials with Carbono of 0.95 % |
Cromo | 0.6 % Show Supplier Material materials with Cromo of 0.6 % |
Hierro | Balance |
Manganeso | 1.1 % Show Supplier Material materials with Manganeso of 1.1 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % |
Wolframio | 0.6 % Show Supplier Material materials with Wolframio of 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Blanking and stamping dies for cutting sheets, threading tools, drills, broaches, gauges, measuring tools, plastic moulds, shear blades, guide rails | |
Heat Treatment | Soft annealing: 800-840°C (Cooling in furnace) - Stress-relief-annealing: 650-700°C (cooling in Furnace), Hardening: 950-980°C and quenching in oil, air or salt bath: 500-550°C |