Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 295 [-] Show Supplier Material materials with Dureza Brinell of 295 [-] | soft annealed |
Dureza Rockwell C | 50 - 54 [-] Show Supplier Material materials with Dureza Rockwell C of 50 - 54 [-] | |
Resistencia a la tracción | 1665 - 1920 MPa Show Supplier Material materials with Resistencia a la tracción of 1665 - 1920 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 1.5 % Show Supplier Material materials with Cromo of 1.5 % |
Hierro | Balance |
Manganeso | 0.7 % Show Supplier Material materials with Manganeso of 0.7 % |
Molibdeno | 0.8 % Show Supplier Material materials with Molibdeno of 0.8 % |
Níquel | 4 % Show Supplier Material materials with Níquel of 4 % |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % |
Vanadio | 0.5 % Show Supplier Material materials with Vanadio of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for cold-shear blades, particularly for cutting scrap, drawing jaws, coining and bending tools | |
Heat Treatment | Soft annealing: 610-650°C (Cooling in furnace) - Stress-relief-annealing: 600°C (cooling in Furnace), Hardening: 880-910°C and quenching in air, oil or salt bath: 180-220°C |