Medidas
Property | Value |
---|---|
Diámetro | 10 - 220 mm Show Supplier Material materials with Diámetro of 10 - 220 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 220 [-] Show Supplier Material materials with Dureza Brinell of 220 [-] | soft annealed |
Dureza Rockwell C | 51 - 59 [-] Show Supplier Material materials with Dureza Rockwell C of 51 - 59 [-] |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for spring collets | |
Heat Treatment | Soft annealing: 680-720°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 820-860°C and quenching in air, oil or salt bath: 180-220°C |