Medidas
Property | Value |
---|---|
Ancho | 1010 mm Show Supplier Material materials with Ancho of 1010 mm |
Espesor | 15 - 200 mm Show Supplier Material materials with Espesor of 15 - 200 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 220 [-] Show Supplier Material materials with Dureza Brinell of 220 [-] | soft annealed |
Dureza Rockwell C | 56 - 60 [-] Show Supplier Material materials with Dureza Rockwell C of 56 - 60 [-] |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.22e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.22e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.32e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.32e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.38e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.38e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.43e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.43e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.47e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.47e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.53e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.53e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 33 W/(m·K) Show Supplier Material materials with Conductividad térmica of 33 W/(m·K) | |
350 °C | 32 W/(m·K) Show Supplier Material materials with Conductividad térmica of 32 W/(m·K) | ||
700 °C | 32.3 W/(m·K) Show Supplier Material materials with Conductividad térmica of 32.3 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.9 % Show Supplier Material materials with Carbono of 0.9 % |
Cromo | 0.4 % Show Supplier Material materials with Cromo of 0.4 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Universally usable, cutting and stamping tools, thread-cutting tools, reamers, gauges, measuring tools, plastic moulds, shear blades, guide rails, ejector pins | |
Heat Treatment | Soft annealing: 680-720°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 790-820°C and quenching in air, oil or salt bath: 180-220°C |