Medidas
Property | Value |
---|---|
Diámetro | 26 - 453 mm Show Supplier Material materials with Diámetro of 26 - 453 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 250 [-] Show Supplier Material materials with Dureza Brinell of 250 [-] | soft annealed |
Dureza Rockwell C | 57 - 63 [-] Show Supplier Material materials with Dureza Rockwell C of 57 - 63 [-] |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 0.000114 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000114 1/K | for 20°C to the mentioned temperature |
150 °C | 0.000116 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000116 1/K | for 20°C to the mentioned temperature | |
200 °C | 0.000117 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000117 1/K | for 20°C to the mentioned temperature | |
250 °C | 0.000119 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000119 1/K | for 20°C to the mentioned temperature | |
300 °C | 0.00012 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00012 1/K | for 20°C to the mentioned temperature | |
350 °C | 0.000121 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000121 1/K | for 20°C to the mentioned temperature | |
400 °C | 0.000123 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000123 1/K | for 20°C to the mentioned temperature | |
450 °C | 0.000124 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000124 1/K | for 20°C to the mentioned temperature | |
500 °C | 0.000126 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 24 W/(m·K) Show Supplier Material materials with Conductividad térmica of 24 W/(m·K) | |
100 °C | 25.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 25.9 W/(m·K) | ||
150 °C | 26.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 26.8 W/(m·K) | ||
200 °C | 27.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 27.1 W/(m·K) | ||
300 °C | 27.4 W/(m·K) Show Supplier Material materials with Conductividad térmica of 27.4 W/(m·K) | ||
400 °C | 27.52 W/(m·K) Show Supplier Material materials with Conductividad térmica of 27.52 W/(m·K) | ||
500 °C | 26.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 26.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 1 % Show Supplier Material materials with Carbono of 1 % |
Cromo | 8 % Show Supplier Material materials with Cromo of 8 % |
Hierro | Balance |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % |
Molibdeno | 1.1 % Show Supplier Material materials with Molibdeno of 1.1 % |
Silicona | 0.9 % Show Supplier Material materials with Silicona of 0.9 % |
Vanadio | 1.6 % Show Supplier Material materials with Vanadio of 1.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting and punching tools including precision cutting tools, threading dies and rolls, rotary shear blades, cold pilger mandrels, strike plates, plastic moulds, coldforming and deep-drawing dies, woodworking tools, cold rolls | |
Heat Treatment | Soft annealing: 830-860°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 1030-1080°C and quenching in air, oil or salt bath: 500-550°C |