Medidas
Property | Value |
---|---|
Diámetro | 10 - 323 mm Show Supplier Material materials with Diámetro of 10 - 323 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 269 [-] Show Supplier Material materials with Dureza Brinell of 269 [-] | annealed |
Dureza Rockwell C | 64 - 66 [-] Show Supplier Material materials with Dureza Rockwell C of 64 - 66 [-] |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20 °C | 32.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 32.8 W/(m·K) |
350 °C | 23.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 23.5 W/(m·K) | |
700 °C | 25.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 25.5 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.9 % Show Supplier Material materials with Carbono of 0.9 % |
Cromo | 4.1 % Show Supplier Material materials with Cromo of 4.1 % |
Hierro | Balance |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % |
Vanadio | 1.9 % Show Supplier Material materials with Vanadio of 1.9 % |
Wolframio | 6.4 % Show Supplier Material materials with Wolframio of 6.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metal-cutting tools for roughing or finishing, shaping tools, woodworking tools, suitable for cold-forming tools | |
Heat Treatment | Soft annealing: 820-860°C (Cooling in furnace) - Stress relief annealing: 630-650°C (Cooling in furnace) - Hardening: 1190-1230°C and quenching in air, oil or salt bath T=530-560°C - Tempering: at least 3 times 530-560°C |