Property | Value | Comment |
---|---|---|
Dureza Brinell | 269 [-] Show Supplier Material materials with Dureza Brinell of 269 [-] | annealed |
Dureza Rockwell C | 64 - 66 [-] Show Supplier Material materials with Dureza Rockwell C of 64 - 66 [-] |
Chemical properties
Property | Value |
---|---|
Carbono | 1.22 % Show Supplier Material materials with Carbono of 1.22 % |
Cromo | 4.1 % Show Supplier Material materials with Cromo of 4.1 % |
Hierro | Balance |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % |
Vanadio | 2.9 % Show Supplier Material materials with Vanadio of 2.9 % |
Wolframio | 6.4 % Show Supplier Material materials with Wolframio of 6.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Taps, reamers, heavy-duty milling cutters, rotary gear shaping and shaving cutters for processing of hard materials, hexagon socket punches and piercing dies for the nut production | |
Heat Treatment | Soft annealing: 820-860°C (Cooling in furnace) - Stress relief annealing: 630-650°C (Cooling in furnace) - Hardening: 1190-1230°C and quenching in air, oil or salt bath T=550°C - Tempering: at least 3 times 540-570°C |