General
Property | Value |
---|---|
Densidad | 7.4 g/cm³ Show Supplier Material materials with Densidad of 7.4 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 59 - 62 [-] Show Supplier Material materials with Dureza Rockwell C of 59 - 62 [-] |
Módulo elástico | 220 GPa Show Supplier Material materials with Módulo elástico of 220 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.11e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.13e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.13e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Supplier Material materials with Azufre of 0.05 % |
Carbono | 2.45 % Show Supplier Material materials with Carbono of 2.45 % |
Cromo | 5.3 % Show Supplier Material materials with Cromo of 5.3 % |
Hierro | Balance |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % |
Molibdeno | 1.3 % Show Supplier Material materials with Molibdeno of 1.3 % |
Silicona | 0.9 % Show Supplier Material materials with Silicona of 0.9 % |
Vanadio | 10 % Show Supplier Material materials with Vanadio of 10 % |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes, screw conveyors |