General
Property | Value |
---|---|
Densidad | 7.1 g/cm³ Show Supplier Material materials with Densidad of 7.1 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 62 - 65 [-] Show Supplier Material materials with Dureza Rockwell C of 62 - 65 [-] |
Módulo elástico | 220 GPa Show Supplier Material materials with Módulo elástico of 220 GPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 4.4 % Show Supplier Material materials with Carbono of 4.4 % | ||
Cobalto | 0.5 % Show Supplier Material materials with Cobalto of 0.5 % | Ni+Co+W | |
Cromo | 13 % Show Supplier Material materials with Cromo of 13 % | ||
Hierro | Balance | ||
Manganeso | 0.9 % Show Supplier Material materials with Manganeso of 0.9 % | ||
Molibdeno | 1.2 % Show Supplier Material materials with Molibdeno of 1.2 % | ||
Níquel | 0.5 % Show Supplier Material materials with Níquel of 0.5 % | Ni+Co+W | |
Silicona | 0.9 % Show Supplier Material materials with Silicona of 0.9 % | ||
Vanadio | 15 % Show Supplier Material materials with Vanadio of 15 % | ||
Wolframio | 0.5 % Show Supplier Material materials with Wolframio of 0.5 % | Ni+Co+W |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes; screw conveyors; knifes for the food industry |