General
Property | Value |
---|---|
Densidad aparente | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Densidad aparente of 3.8 - 4.6 g/cm³ |
Rango de tamaño de partículas | 10 - 53 µm Show Supplier Material materials with Rango de tamaño de partículas of 10 - 53 µm |
Mecánica
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 165 J Show Supplier Material materials with Charpy impact energy, V-notch of 165 J | |
Elongación | 45 % Show Supplier Material materials with Elongación of 45 % | A5 |
Límite elástico | 440 - 540 MPa Show Supplier Material materials with Límite elástico of 440 - 540 MPa | RP02 |
Resistencia a la tracción | 520 - 620 MPa Show Supplier Material materials with Resistencia a la tracción of 520 - 620 MPa |
Magnético
Property | Value | Comment |
---|---|---|
Permeabilidad magnética relativa | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Flujo de Hall | 12 - 20 s/50g Show Supplier Material materials with Flujo de Hall of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 17 % Show Supplier Material materials with Cromo of 17 % |
Hierro | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 2 % Show Supplier Material materials with Molibdeno of 2 % |
Níquel | 13 % Show Supplier Material materials with Níquel of 13 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Corrosion properties | In printed condition Prindur® 4404 is corrosion resistant according to SEP 1877 Method II (intergranular corrosion resistance test) and ASTM G48 Method E (pitting corrosion resistance test). | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® 4404 can be processed on LPBF systems. The process parameters are similar to those of 1.4404/316L. |