General
Property | Value |
---|---|
Densidad aparente | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Densidad aparente of 3.8 - 4.6 g/cm³ |
Rango de tamaño de partículas | 20 - 53 µm Show Supplier Material materials with Rango de tamaño de partículas of 20 - 53 µm |
Mecánica
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 100 J Show Supplier Material materials with Charpy impact energy, V-notch of 100 J | |
Elongación | 35 % Show Supplier Material materials with Elongación of 35 % | A5 |
Límite elástico | 660 - 760 MPa Show Supplier Material materials with Límite elástico of 660 - 760 MPa | RP02 |
Resistencia a la tracción | 920 - 1030 MPa Show Supplier Material materials with Resistencia a la tracción of 920 - 1030 MPa |
Magnético
Property | Value | Comment |
---|---|---|
Permeabilidad magnética relativa | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Flujo de Hall | 12 - 20 s/50g Show Supplier Material materials with Flujo de Hall of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cobalto | 0.5 % Show Supplier Material materials with Cobalto of 0.5 % |
Cromo | 22 % Show Supplier Material materials with Cromo of 22 % |
Hierro | 5 % Show Supplier Material materials with Hierro of 5 % |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % |
Molibdeno | 9 % Show Supplier Material materials with Molibdeno of 9 % |
Niobio | 3.5 % Show Supplier Material materials with Niobio of 3.5 % |
Níquel | Balance |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® Ni625 can be processed on LPBF systems. The process parameters are similar to those of alloy 625. Please contact us for further information. |