General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Densidad aparente | 4.63 g/cm³ Show Supplier Material materials with Densidad aparente of 4.63 g/cm³ |
Rango de tamaño de partículas | 10 - 45 µm Show Supplier Material materials with Rango de tamaño de partículas of 10 - 45 µm |
Mecánica
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 22 J Show Supplier Material materials with Charpy impact energy, V-notch of 22 J | |
Dureza Rockwell C | 27 [-] Show Supplier Material materials with Dureza Rockwell C of 27 [-] | |
Elongación | 27 % Show Supplier Material materials with Elongación of 27 % | A5 |
Límite elástico | 630 MPa Show Supplier Material materials with Límite elástico of 630 MPa | RP02 |
Resistencia a la tracción | 1080 MPa Show Supplier Material materials with Resistencia a la tracción of 1080 MPa |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 1.05e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.05e-05 1/K |
Rheological Properties
Property | Value |
---|---|
Flujo de Hall | 16 s/50g Show Supplier Material materials with Flujo de Hall of 16 s/50g |
Chemical properties
Property | Value |
---|---|
Carbono | 0.14 % Show Supplier Material materials with Carbono of 0.14 % |
Cobalto | Balance |
Cromo | 28 % Show Supplier Material materials with Cromo of 28 % |
Hierro | 0.75 % Show Supplier Material materials with Hierro of 0.75 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 6 % Show Supplier Material materials with Molibdeno of 6 % |
Nitrógeno | 0.25 % Show Supplier Material materials with Nitrógeno of 0.25 % |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for the production of CoCrMo implants | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® CoCrF75 can be processed on LPBF systems. |