General
Property | Value |
---|---|
Densidad aparente | 4.3 g/cm³ Show Supplier Material materials with Densidad aparente of 4.3 g/cm³ |
Rango de tamaño de partículas | 10 - 53 µm Show Supplier Material materials with Rango de tamaño de partículas of 10 - 53 µm |
Mecánica
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 50 J Show Supplier Material materials with Charpy impact energy, V-notch of 50 J | |
Dureza Rockwell C | 35 [-] Show Supplier Material materials with Dureza Rockwell C of 35 [-] | |
Elongación | 30 % Show Supplier Material materials with Elongación of 30 % | A5 |
Límite elástico | 915 MPa Show Supplier Material materials with Límite elástico of 915 MPa | RP02 |
Resistencia a la tracción | 1120 MPa Show Supplier Material materials with Resistencia a la tracción of 1120 MPa |
Magnético
Property | Value | Comment |
---|---|---|
Permeabilidad magnética relativa | 1 [-] Show Supplier Material materials with Permeabilidad magnética relativa of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Flujo de Hall | 16.8 s/50g Show Supplier Material materials with Flujo de Hall of 16.8 s/50g |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 1 % Show Supplier Material materials with Carbono of 1 % | N+C | |
Cromo | 18 % Show Supplier Material materials with Cromo of 18 % | ||
Hierro | Balance | ||
Manganeso | 21 % Show Supplier Material materials with Manganeso of 21 % | ||
Molibdeno | 2 % Show Supplier Material materials with Molibdeno of 2 % | ||
Nitrógeno | 1 % Show Supplier Material materials with Nitrógeno of 1 % | N+C | |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | The properties of Printdur® HSA offer a wide range of applications in mechanical engineering, e.g. food and chemical industry, pump components, the power plant industry or the automotive industy. | |
Corrosion properties | In printed condition Prindur® HSA is corrosion resistant according to SEP 1877 Method II (intergranular corrosion resistance test) and ASTM G48 Method E (pitting corrosion resistance test). | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® HSA can be processed on LPBF systems. The process parameters are similar to those of 316L. Please contact us for further information. |