Property | Value |
---|---|
Densidad aparente | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Densidad aparente of 3.8 - 4.6 g/cm³ |
Rango de tamaño de partículas | 20 - 53 µm Show Supplier Material materials with Rango de tamaño de partículas of 20 - 53 µm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Rockwell C | 37 [-] Show Supplier Material materials with Dureza Rockwell C of 37 [-] | |
Elongación | 65 % Show Supplier Material materials with Elongación of 65 % | A5 |
Límite elástico | 900 - 950 MPa Show Supplier Material materials with Límite elástico of 900 - 950 MPa | RP02 |
Resistencia a la tracción | 980 - 1080 MPa Show Supplier Material materials with Resistencia a la tracción of 980 - 1080 MPa |
Rheological Properties
Property | Value |
---|---|
Flujo de Hall | 12 - 20 s/50g Show Supplier Material materials with Flujo de Hall of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % |
Cobalto | 13.5 % Show Supplier Material materials with Cobalto of 13.5 % |
Hierro | Balance |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % |
Níquel | 18 % Show Supplier Material materials with Níquel of 18 % |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Manufacturing | |
Heat Treatment | Solution annealed (vacuum, 850°C/ 1h/ gas quenching) and ageing (480°C, 4h, air cooling) | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Der Printdur® Powderfort can be processed on LPBF systems. The process parameters are similar to those of 1.2709. Please contact us for further information. |