Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 40 J Show Supplier Material materials with Charpy impact energy, V-notch of 40 J | |
Dureza Rockwell C | 44 [-] Show Supplier Material materials with Dureza Rockwell C of 44 [-] | |
Elongación | 10 % Show Supplier Material materials with Elongación of 10 % | A5 |
Límite elástico | 1220 MPa Show Supplier Material materials with Límite elástico of 1220 MPa | RP02 |
Resistencia a la tracción | 1500 MPa Show Supplier Material materials with Resistencia a la tracción of 1500 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.22 % Show Supplier Material materials with Carbono of 0.22 % |
Cromo | 1 % Show Supplier Material materials with Cromo of 1 % |
Manganeso | 1.4 % Show Supplier Material materials with Manganeso of 1.4 % |
Molibdeno | 1 % Show Supplier Material materials with Molibdeno of 1 % |
Silicona | 0.8 % Show Supplier Material materials with Silicona of 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Bainidur® AM can be processed on LPBF systems |