General
Property | Value |
---|---|
Densidad | 7.7 g/cm³ Show Supplier Material materials with Densidad of 7.7 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Diámetro | 100 mm Show Supplier Material materials with Diámetro of 100 mm | max. |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 223 [-] Show Supplier Material materials with Dureza Brinell of 223 [-] | annealed |
Elongación | 12 - 15 % Show Supplier Material materials with Elongación of 12 - 15 % | A5 |
Estricción | 25 - 40 % Show Supplier Material materials with Estricción of 25 - 40 % | |
Límite elástico | 400 - 510 MPa Show Supplier Material materials with Límite elástico of 400 - 510 MPa | |
Módulo elástico | 210 GPa Show Supplier Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 640 - 880 MPa Show Supplier Material materials with Resistencia a la tracción of 640 - 880 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 470 J/(kg·K) Show Supplier Material materials with Calor específico of 470 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.25e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.25e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.33e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.33e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.39e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.39e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 42.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 42.6 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 1.9e-07 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.9e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % |
Carbono | 0.5 - 0.57 % Show Supplier Material materials with Carbono of 0.5 - 0.57 % |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % |
Hierro | Balance |
Manganeso | 0.4 - 0.7 % Show Supplier Material materials with Manganeso of 0.4 - 0.7 % |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % |
Technological properties
Property | ||
---|---|---|
Application areas | It mainly used in the automotive industry such as axle parts. | |
Heat Treatment | Normalizing 830-860°C (Air), Soft annealing: 650-700°C (slow cooling), Quenching: 805-835°C (Water) or 815-845°C (Oil, Polymer), Tempering: 550-660°C (Oil, Polymer, Water) | |
Hot forming | It is formable at 850-1050°C | |
Processing history | Quenched and Tempered | |
Welding | It is usually not weldable and should will not be used in welded constructions. |