General
Property | Value | Comment |
---|---|---|
Densidad | 1.05 g/cm³ Show Supplier Material materials with Densidad of 1.05 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 30.0 % Show Supplier Material materials with Elongación of 30.0 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 250.0 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250.0 J/m | ASTM D256 |
Módulo de flexión | 2.35 GPa Show Supplier Material materials with Módulo de flexión of 2.35 GPa | ASTM D790 |
Módulo elástico | 2.15 GPa Show Supplier Material materials with Módulo elástico of 2.15 GPa | ASTM D638 |
Resistencia a la flexión | 67.35 MPa Show Supplier Material materials with Resistencia a la flexión of 67.35 MPa | ASTM D790 |
Resistencia a la tracción | 42.5 MPa Show Supplier Material materials with Resistencia a la tracción of 42.5 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de fusión | 180.0 - 200.0 °C Show Supplier Material materials with Temperatura de fusión of 180.0 - 200.0 °C | ISO 3146-C | |
Temperatura de reblandecimiento Vicat | 94 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 94 °C | ASTM D1525 | |
Inflamabilidad | UL-94 1/16‘ HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | ASTM D955 |
Velocidad de flujo de la masa derretida | 44.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 44.0 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | The strength, flexibility, machinability and high-temperature resistance of ABS often makes it the plastic preferred by engineers and people intending to use plastic in a mechanical context. | |
Certifications | Extrudr ABS can be used in applications for direct/indirect food contact under the FDA regulation | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |