General
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 100 % Show Supplier Material materials with Bio-based content of 100 % | ||
Densidad | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ASTM D882 |
Resistencia a la tracción | 23.0 °C | 61 MPa Show Supplier Material materials with Resistencia a la tracción of 61 MPa | ASTM D882 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 190 - 200 °C Show Supplier Material materials with Temperatura de fusión of 190 - 200 °C | ISO 3146-C |
Temperatura de reblandecimiento Vicat | 60 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 60 °C | ISO 306 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ISO 294-4 |
Velocidad de flujo de la masa derretida | 6.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 6.5 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | PLA is used to make an increasingly wide variety of products. PLA can be used in rapid prototyping, architecture, food applications, toys and outdoor novelties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |