General
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 90 % Show Supplier Material materials with Bio-based content of 90 % | ||
Densidad | 23.0 °C | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | ISO 527 |
Módulo de flexión | 23.0 °C | 7.12 GPa Show Supplier Material materials with Módulo de flexión of 7.12 GPa | ISO 527 |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.6 kJ/m² | ISO 179-1/1 eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 82 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 82 kJ/m² | ISO 179-1/1 eU |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 115 °C | ISO 75/B |
Temperatura de flexión bajo carga | 115 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 115 °C | |
Temperatura de fusión | 190 - 240 °C Show Supplier Material materials with Temperatura de fusión of 190 - 240 °C | ISO 3146-C |
Temperatura de reblandecimiento Vicat | 165 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 165 °C | ISO 306 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | GreenTEC PRO Carbon is designed for extreme industrial use. It has very good mechanical and thermal properties | |
Fillers | 10% Carbon Fiber | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |