General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 19 % Show Supplier Material materials with Elongación of 19 % | ISO 527 |
Módulo de flexión | 23.0 °C | 2.65 GPa Show Supplier Material materials with Módulo de flexión of 2.65 GPa | ISO 527 |
Módulo elástico | 23.0 °C | 2.65 GPa Show Supplier Material materials with Módulo elástico of 2.65 GPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 49 MPa Show Supplier Material materials with Resistencia a la tracción of 49 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | ISO 179-1/1 eA |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 64 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 64 kJ/m² | ISO 178 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 150 - 170 °C Show Supplier Material materials with Temperatura de fusión of 150 - 170 °C | ISO 3146-C |
Temperatura de reblandecimiento Vicat | 60 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 60 °C | ISO 306 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ISO 294-4 |
Velocidad de flujo de la masa derretida | 3.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.5 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Biocompounds with high impact resistance and a matte surface are suitable for industrial use, rapid prototyping, architecture, food applications, toys and outdoor novelties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |