Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 14 % Show Supplier Material materials with Elongación of 14 % | ISO 527 |
Módulo de flexión | 23.0 °C | 3.3 GPa Show Supplier Material materials with Módulo de flexión of 3.3 GPa | ISO 527 |
Resistencia a la tracción | 23.0 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 19 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 19 kJ/m² | ISO 179-1/1 eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 218 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 218 kJ/m² | ISO 179-1/1 eU |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 47 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 47 °C | ISO 75/B |
Temperatura de flexión bajo carga | 47 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 47 °C | |
Temperatura de fusión | 180 - 200 °C Show Supplier Material materials with Temperatura de fusión of 180 - 200 °C | ISO 3146-C |
Temperatura de reblandecimiento Vicat | 115 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 115 °C | ISO 306 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | ISO 294-4 |
Velocidad de flujo de la masa derretida | 3.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.5 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | GreenTEC is designed for industrial use. It has good mechanical and thermal properties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |