General
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 100 % Show Supplier Material materials with Bio-based content of 100 % | ||
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ISO 2781 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.9 % Show Supplier Material materials with Elongación of 6.9 % | ISO 527 |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ISO 527 |
Módulo elástico | 23.0 °C | 1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 30.1 MPa Show Supplier Material materials with Resistencia a la flexión of 30.1 MPa | ISO 527 |
Resistencia a la tracción | 23.0 °C | 34 MPa Show Supplier Material materials with Resistencia a la tracción of 34 MPa | ISO 527 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 51 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 51 °C | ISO 75/B |
Temperatura de flexión bajo carga | 51 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 51 °C | |
Temperatura de reblandecimiento Vicat | 58 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 58 °C | ISO 306 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Pearl is characterized by its uniquely silky-smooth surface. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |