Description

This material produced from alloy EN AW 7021 (AlZn5.5Mg1.5) in a vertical continuous casting process closes the gap between medium and high-strength aluminum materials, the latter of which are often overqualified. G.AL® C330 is characterized by a very fine and homogenous structure, very low microporosity, excellent machinability and very high strength. G.AL® C330 is manufactured in material temper T79, which is reflected in the low-stress properties and dimensional stability unique in this strength class.

Equivalent Materials

Los datos sobre este material han sido proporcionados por Gleich Aluminum.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

2.8 g/cm³

Show Supplier Material materials with Densidad of 2.8 g/cm³

Rugosidad superficial

0.4 μm

Show Supplier Material materials with Rugosidad superficial of 0.4 μm

Medidas

PropertyValue

Ancho

1500 mm

Show Supplier Material materials with Ancho of 1500 mm

Dimensions

Standard stock sizes: 1540mm x 3048mm and 10-50mm in thickness

Mecánica

PropertyTemperatureValueComment

Dureza Brinell (HBW)

23.0 °C

110 - 120 [-]

Show Supplier Material materials with Dureza Brinell (HBW) of 110 - 120 [-]

Test method: 2.5/62.5

Elongación A5

23.0 °C

2.5 - 4.5 %

Show Supplier Material materials with Elongación A5 of 2.5 - 4.5 %

Límite elástico Rp 0,2

23.0 °C

290 - 340 MPa

Show Supplier Material materials with Límite elástico Rp 0,2 of 290 - 340 MPa

Módulo elástico

23.0 °C

70 GPa

Show Supplier Material materials with Módulo elástico of 70 GPa

Resistencia a la tracción

23.0 °C

320 - 380 MPa

Show Supplier Material materials with Resistencia a la tracción of 320 - 380 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

23.0 °C

875 J/(kg·K)

Show Supplier Material materials with Calor específico of 875 J/(kg·K)

Coeficiente de dilatación térmica

23.0 °C

2.3E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K

Conductividad térmica

23.0 °C

125 - 155 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 125 - 155 W/(m·K)

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

23.0 °C

2.10E+7 - 2.40E+7 S/m

Show Supplier Material materials with Conductividad eléctrica of 2.10E+7 - 2.40E+7 S/m

Technological properties

Property
Other

Heat treatable alloy

Processing history

Temper: T79, solution heat treated, quenched, artificially aged